INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Structural thermoplastic

Structural thermoplastic

Structural thermoplastic

(OP)


Looking for reccommendations for a structural
thermoplastic. Must meet
or exceed these properties:

-Weldable with high weld strength
-Tensile strength = 30,000 psi
-flexural strength = 50,000 psi
-IZOD impact, notched = 5 ft-lb/in
compressive strength = 30,000 psi
normal op temp = -40 to 200 F

Any help is greatly welcomed.

RE: Structural thermoplastic

Celstran is a Ticona product line of fiber reinforced thermoplastic injection molding materials. A Celstran material which meets your requirements is PA66-GF50-02. This is a nylon 66, 50% long glass fiber by weight with the following properties:

TS: -40°F = 49,700 psi
72°F = 40,600 psi
300°F = 22,200 psi

FS: -40°F = 66,000 psi
72°F = 59,100 psi
300°F = 31,000 psi

IZOD, notched: -40°F = 11.6 ft-lbs
72°F = 11.5 ft-lbs
300°F = 13.8 ft-lbs

Compressive Strength: 44,900 psi

For assistance with application development, please call Mike Wesley at (507) 457-4062.

Good luck.





Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members! Already a Member? Login


Resources

Design for Additive Manufacturing (DfAM)
Examine how the principles of DfAM upend many of the long-standing rules around manufacturability - allowing engineers and designers to place a part’s function at the center of their design considerations. Download Now
Taking Control of Engineering Documents
This ebook covers tips for creating and managing workflows, security best practices and protection of intellectual property, Cloud vs. on-premise software solutions, CAD file management, compliance, and more. Download Now

Close Box

Join Eng-Tips® Today!

Join your peers on the Internet's largest technical engineering professional community.
It's easy to join and it's free.

Here's Why Members Love Eng-Tips Forums:

Register now while it's still free!

Already a member? Close this window and log in.

Join Us             Close