Recently we conducted a metal test analysis to prove that we have raw circulating sea water pump with the right material as per ASTM No. B148 AL985. Following is the test result
Cu: 86.07%
AL: 9.06%
Fe: 4.00%
Ni: 0.69%
Mn:0.18%
Pb:0.003%
Si:<0.001%
Can anybody help me to identify wether the test result meet the ASTM spec. Thanks.
 