INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

hardness at 5/8 inches depth to the face

hardness at 5/8 inches depth to the face

hardness at 5/8 inches depth to the face

(OP)
Hi,

I have a 13 inches wheel by 3 inches thickness that got an heat treatment.  I want to know if it's possible to get the hardness at 5/8 inches depth to the face, without destroy the pieces.

I don't have a jominy test or a sampler.

Maybe a magnetics or ultrasonic testing can do?
Replies continue below

Recommended for you

RE: hardness at 5/8 inches depth to the face

What kind of heat treatment was performed? Through hardening or some form of surface treatment (flame, induction?)

RE: hardness at 5/8 inches depth to the face

The depth of hardening achieved would depend on the material grade of the wheel and the type of heat treatment performed. However,irrespective of the these it would be impossible to verify the hardness at a specific depth on the actual component without cutting samples from the component for cross a section hardness survey. If this is not possible then you could recreate the heat treatment on test piece using the same material grade. This could then be used to verify the hardness levels at the depth you require.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members! Already a Member? Login



News


Close Box

Join Eng-Tips® Today!

Join your peers on the Internet's largest technical engineering professional community.
It's easy to join and it's free.

Here's Why Members Love Eng-Tips Forums:

Register now while it's still free!

Already a member? Close this window and log in.

Join Us             Close