material name standard s355j2 or en 1.0577 1

Status
Not open for further replies.

IvanNX

Mechanical
Joined
Jun 9, 2005
Messages
267
Location
SE
Can somebody give me links or just an explanation of the difference between naming material s355j2 or en 1.0577... what naming belongs to what standard and are there any rules on how to use these names?

Thank you.

_____________________________
Enjoy your work and have fun!
 
EN 10025-2 : S355J2
Werkstoffnummer : 1.0577

In construction, EN 10025-X designations are commonly used.
For stainless or exotic materials, the werkstoffnummer is often used.

See also ISO TR 20172/20173/20174
 