Is there a commonly accepted test for a existing mat or slab on grade?
 
Replies continue below

Recommended for you

ACI 318 has section 27 (318-14 and later).


 
Oops - sorry - I quickly and not-carefully read you question as a suspended slab.

No on-grade load test that I'm aware of unless the civil engineers doing pavement design know a method.

 