What is the best way to melt down metal that has 3000° degree celsius melting point at medium scale backyard foundry
 
Replies continue below

Recommended for you

There is no way you are getting to 3000°C. You are not getting to 3000°F in a backyard foundry.

Bob
 
Build an arc furnace?

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed
 