NACE TM0177 METHOD B TEST
NACE TM0177 METHOD B TEST
(OP)
Hello, please let us know the test method about NACE TM 0177 method b for pipe sample and procedure for the same
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Contact USThanks. We have received your request and will respond promptly. Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting Guidelines |
NACE TM0177 METHOD B TEST
|
Join your peers on the Internet's largest technical engineering professional community.
It's easy to join and it's free.
Here's Why Members Love Eng-Tips Forums:
Register now while it's still free!
Already a member? Close this window and log in.
RE: NACE TM0177 METHOD B TEST
methods A, B, etc. in ASTM TM 0177 are related to the loading type : method B is the "bent beam" method that differs from "method A, tensile".
please have a look in the document you make reference to (NACE TM 0177)
regards
RE: NACE TM0177 METHOD B TEST
DHURJATI SEN
RE: NACE TM0177 METHOD B TEST
Eng-Tips will not be a vehicle for trafficing stolen Western Documents ...
You will have to find some amoral Third-World website that has no problem doing this
MJCronin
Sr. Process Engineer
RE: NACE TM0177 METHOD B TEST
RE: NACE TM0177 METHOD B TEST
The B method was put in by Shell when I was on the committee in the 80's and 90's. At that time I don't recall any company but Shell using it routinely. At that time people who wrote the NACE documents got no compensation from NACE. NACE Staff did the editorial and publishing work.
t