Feb 3, 2021 #1 NDT3RICH Petroleum Joined Aug 19, 2015 Messages 12 Location US I'm sure this is fairly common, but I am really curious as to what the tensile specimens looked like. I only have access to the WPS, and it seems like there are way too many cracking issues for my liking with this combination.
I'm sure this is fairly common, but I am really curious as to what the tensile specimens looked like. I only have access to the WPS, and it seems like there are way too many cracking issues for my liking with this combination.
Feb 3, 2021 #2 0707 Petroleum Joined Jun 25, 2001 Messages 3,446 Location PT 6011 and 7018 is the usual option. luis Upvote 0 Downvote
Feb 3, 2021 #3 weldstan Materials Joined Jun 24, 2011 Messages 2,808 Location US For pipelining it used to be E6010 all the way with downhill progression. Don't know why one would use E8010 for such low strength material. Upvote 0 Downvote
For pipelining it used to be E6010 all the way with downhill progression. Don't know why one would use E8010 for such low strength material.