I'm sure this is fairly common, but I am really curious as to what the tensile specimens looked like. I only have access to the WPS, and it seems like there are way too many cracking issues for my liking with this combination.
 
Replies continue below

Recommended for you

6011 and 7018 is the usual option.

luis
 
For pipelining it used to be E6010 all the way with downhill progression. Don't know why one would use E8010 for such low strength material.
 