I have a query. Is it possible to have the below properties in a Xm-19 Bar ?
YS ≥ 850 Mpa
TS ≥ 1000 Mpa
Kv ≥ 45 (196°C)
In case the bar is strain hardened, the required Kv properties would not be achievable ?
Thanks
I have a query. Is it possible to have the below properties in a Xm-19 Bar ?
YS ≥ 850 Mpa
TS ≥ 1000 Mpa
Kv ≥ 45 (196°C)
In case the bar is strain hardened, the required Kv properties would not be achievable ?
Thanks
RE: XM-19 (UNS20910 HS) Round Bar
RE: XM-19 (UNS20910 HS) Round Bar
RE: XM-19 (UNS20910 HS) Round Bar
You know that you could buy some pieces off the shelf to test?
Aqumet.com
This ia used as boat prop shafting and you could buy short pieces.
= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed