Aug 20, 2020 #1 Surchi Materials Joined Sep 12, 2019 Messages 2 Location IN How do we check Hardness values for Graphite Block - Is it Rockwell C scale or Rockwell B scale. Which is better
How do we check Hardness values for Graphite Block - Is it Rockwell C scale or Rockwell B scale. Which is better
Aug 20, 2020 #2 EdStainless Materials Joined May 20, 2004 Messages 16,375 Location Waukesha WI USA What is the spec? What does it say? = = = = = = = = = = = = = = = = = = = = P.E. Metallurgy, consulting work welcomed Upvote 0 Downvote
What is the spec? What does it say? = = = = = = = = = = = = = = = = = = = = P.E. Metallurgy, consulting work welcomed
Aug 23, 2020 #3 Dhurjati Sen Materials Joined Dec 14, 2017 Messages 1,005 Location IN Rockwell L perhaps. Check the standard as mentioned below for more...... ASTM C748 - 20 Standard Test Method for Rockwell Hardness of Graphite Materials DHURJATI SEN Kolkata, India Upvote 0 Downvote
Rockwell L perhaps. Check the standard as mentioned below for more...... ASTM C748 - 20 Standard Test Method for Rockwell Hardness of Graphite Materials DHURJATI SEN Kolkata, India
Sep 7, 2020 Thread starter #4 Surchi Materials Joined Sep 12, 2019 Messages 2 Location IN Thanks for the inputs Upvote 0 Downvote