WE ARE IN THE PROCESS OF MAKING A MAGNETIZER FOR MAGNETIZING ARC TYPE BONDED NDFEB MAGNETS.BUT WE COULD REACH ONLY 80%FLUX LEVEL IRRESPECTIVE OF APPLYING MAXIMUM MAGNETIZATION FORCE.IS THERE ANY CRITERIA LIKE SHAPE OR FIXTURE CONSIDERATION THAT AFFECT THE FLUX VALUE OR LIMITING THE SATURATION POINT.ANY LED WILL BE HELPFUL
 