Dear to all ,we are processing Rivet 1018 -annealing ,my requirement is 130-170 HB ,But result come to 1 job 130-160 HB,Lot of variation?Please suggest Cycle.
 
Replies continue below

Recommended for you

What are you using?
Time, temp, and atmosphere.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube
 