Sep 12, 2019 #1 dyani Materials Joined Sep 12, 2019 Messages 1 Location IN Dear to all ,we are processing Rivet 1018 -annealing ,my requirement is 130-170 HB ,But result come to 1 job 130-160 HB,Lot of variation?Please suggest Cycle.
Dear to all ,we are processing Rivet 1018 -annealing ,my requirement is 130-170 HB ,But result come to 1 job 130-160 HB,Lot of variation?Please suggest Cycle.
Sep 12, 2019 #2 EdStainless Materials Joined May 20, 2004 Messages 16,357 Location Waukesha WI USA What are you using? Time, temp, and atmosphere. = = = = = = = = = = = = = = = = = = = = P.E. Metallurgy, Plymouth Tube Upvote 0 Downvote
What are you using? Time, temp, and atmosphere. = = = = = = = = = = = = = = = = = = = = P.E. Metallurgy, Plymouth Tube