stainless steel 17-4 chloride resistance data

Status
Not open for further replies.

Joe Greulich

Materials
Feb 26, 2019
1
Am looking for a website that has data on chloride and sulfate resistance, to evaluate effects of corrosion. Most of the information I can only says has excellent corrosion data, not actual numbers
 
Replies continue below

Recommended for you

Are you after pitting resistance or cracking resistance?
The HT condition matters a lot, for both factors.
In general 17-4 has so-so corrosion resistance.
No as good as good of pitting resistance as 304, and serious environmental cracking issues unless you are in a H11 or 1150 condition.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube
 