INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Contact US

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Staking Tool Material for Steel Parts

Staking Tool Material for Steel Parts

Staking Tool Material for Steel Parts

(OP)
What material do people use for Impact Staking steel parts? We used some 4140 and the part wears pretty quickly. It was quenched and tempered to 46HRC.

We used some S7 also, quenched and tempered to 46HRC and that wore out even faster.

Suggestions? I'm thinking 300m but I thought maybe there was a better go to material.

RE: Staking Tool Material for Steel Parts

I guess it depends on the geometry of the punch and the level of shock in the process, but I'd try plain old A-2 @ C60 give or take.

RE: Staking Tool Material for Steel Parts

(OP)
Any other suggestions?

RE: Staking Tool Material for Steel Parts

Drill rod, O1, or 1095 and harden and temper to Rockwell 60C.

Ted

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members! Already a Member? Login



News


Close Box

Join Eng-Tips® Today!

Join your peers on the Internet's largest technical engineering professional community.
It's easy to join and it's free.

Here's Why Members Love Eng-Tips Forums:

Register now while it's still free!

Already a member? Close this window and log in.

Join Us             Close