AWD D1.5- WPS Qualification Question

Status
Not open for further replies.

newweldeng09

Mechanical
Joined
Oct 31, 2008
Messages
84
Location
US
I am qualifying two production welds. Weld No. 1 is a CJP double-bevel groove meeting B-U5-GF of Fig. 2.4. Weld No. 2 is a PJP square butt weld that does not meet any of the joints in Fig. 2.5. Does the CJP groove weld qualification qualify the PJP groove weld qualification per Par. 5.9.1 or is a separate qualification required for the PJP groove weld as indicated in Par. 5.12?

 
Commentary for Par. 5.9.1 provided an answer to this question.
 