INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Related Articles

Jobs

ASTM A1011 Gr.33 and DIN S355JR

ASTM A1011 Gr.33 and DIN S355JR

ASTM A1011 Gr.33 and DIN S355JR

(OP)
Hi! I would like to ask if DIN S355JR and ASTM A1011 Gr.33 are equivalents. I have specified in my requirement that I need ASTM A1011 Gr.33 plates and one supplier offered DIN S355JR stating that these are the same. Please help me out on this one. Thanks!

RE: ASTM A1011 Gr.33 and DIN S355JR

Moin Moin dr. stray217

I know, for what you need this Part:
Steelname Werkstoffnr Norm EN France Britania Swenska USA Czech Russia Japan China Italy India Spain Hungary Poland Turkey
EStE 355 1.1106 EN 10028-3 P 355NL2         FE 510-2KG   52 E   
P 355N 1.0562 EN 10028-3  A 510 AP 50 D 2106 A 633-C, A 516-65  15 GF SM 490A, B 16 MnR    P 355NB 18 G2A  
P 355NB 1.0557 EN 10120  BS 4      SG 365  Fe E35KR      
P 355NH 1.0565 EN 10222-4, EN 10028-3  A 510 AP  2106 A 737-B     Fe 510-2KW      
P 355NL1 1.0566 EN 10028-3  A 510 FP 1 490 225 2107  11503    Fe 510-1KG


Vessel, Pipe, Feinkornbaustahl   
  
But this is better in the near as the S 355JR.
Baustahl, Bridge

C ~ 0,2, Mn ~ 1.6, Si ~ 0.55
Tensile 510 - 680, Yield ~ 355

And finally the ASTM:

A 1011-SS-33  0,25 0,9  0,2 0,15 0,06 0,025 0,008  0,008 0,035 0,04   0,2  360 230

Hope this help a littlebit
 

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources


Close Box

Join Eng-Tips® Today!

Join your peers on the Internet's largest technical engineering professional community.
It's easy to join and it's free.

Here's Why Members Love Eng-Tips Forums:

Register now while it's still free!

Already a member? Close this window and log in.

Join Us             Close