Hi! I would like to ask if DIN S355JR and ASTM A1011 Gr.33 are equivalents. I have specified in my requirement that I need ASTM A1011 Gr.33 plates and one supplier offered DIN S355JR stating that these are the same. Please help me out on this one. Thanks!
 
Moin Moin dr. stray217

I know, for what you need this Part:
Steelname Werkstoffnr Norm EN France Britania Swenska USA Czech Russia Japan China Italy India Spain Hungary Poland Turkey
EStE 355 1.1106 EN 10028-3 P 355NL2 FE 510-2KG 52 E
P 355N 1.0562 EN 10028-3 A 510 AP 50 D 2106 A 633-C, A 516-65 15 GF SM 490A, B 16 MnR P 355NB 18 G2A
P 355NB 1.0557 EN 10120 BS 4 SG 365 Fe E35KR
P 355NH 1.0565 EN 10222-4, EN 10028-3 A 510 AP 2106 A 737-B Fe 510-2KW
P 355NL1 1.0566 EN 10028-3 A 510 FP 1 490 225 2107 11503 Fe 510-1KG


Vessel, Pipe, Feinkornbaustahl

But this is better in the near as the S 355JR.
Baustahl, Bridge

C ~ 0,2, Mn ~ 1.6, Si ~ 0.55
Tensile 510 - 680, Yield ~ 355

And finally the ASTM:

A 1011-SS-33 0,25 0,9 0,2 0,15 0,06 0,025 0,008 0,008 0,035 0,04 0,2 360 230

Hope this help a littlebit
 