I was just wondering if anyone has a complete data set for the target mass loss for the coupons in GM9540P. The table is incomplete and calculating the target losses from the end of test mass loss seems a bit confusing to me. If anyone has any info or any tips on figuring out my little dilemma, it would be much appreciated to hear from you!

Thanks,
Paul T. Collins