I have a hole with 3/4 14 npsf thread and verify with L1 and L3 gage, when I veryfied with L1 gage is ok, and when it veryfied with L3, pass through all the hole, what you think is the problem, conicity, big diameter before threaded
 
threads refence off the pitch diameter, not the minor (inner) diameter
 