Jun 23, 2009 #1 fazel2 Materials Joined Nov 21, 2008 Messages 16 Location IR Can we use pqr of CJP V groove type for other groove type(e.g double V- groove or single bevel and... ( square- groove is excluded)) in WPS of CJP groove welds ?
Can we use pqr of CJP V groove type for other groove type(e.g double V- groove or single bevel and... ( square- groove is excluded)) in WPS of CJP groove welds ?
Jun 23, 2009 #2 DVWE Petroleum Joined Apr 5, 2007 Messages 2,374 Location US Yes. The requirements are a little different between AWS D1.1 and ASME Section IX. You can reference Table 4.5 - General section in D1.1 for groove type. Upvote 0 Downvote
Yes. The requirements are a little different between AWS D1.1 and ASME Section IX. You can reference Table 4.5 - General section in D1.1 for groove type.