Yeoh Model doesn't run in Algor

Status
Not open for further replies.

muammeryazici

Mechanical
Feb 26, 2009
1
Hi,
I try to constitute the yeoh material model in Algor for various rubbers.
And i determined constants from test datas.
But I cant make run yeoh model that i found its constant.
c1=0,6 c2=0,002 c3=0,005 K1,2,3=1000

I constituted for mooney model that have run.

best regards...