Hi,

Please help me!
I recieved an RFQ, wich include some EPDM material.
Due I'm not a master on these type materials (maybe my english is not so good too - I'm working on it)I ask for your help!

EPDM to ASTM D200 4MAA 510 A13 B13 C12 - What does it mean?
Can you advise me a named material?

Thanks
Gagar
 
It took me 30 seconds on google to find a significant amount of information.

Give it a try before you ask others to invest time.

What is an RFQ other than another TLA

Regards

eng-tips, by professional engineers for professional engineers
Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
The standard is ASTM D2000 not D200. EPDM is a type of thermoset rubber (elastomer).
 
.
Etylenepropylenediene rubber (EPDM) "hence the acronym"
.
* Excellent resistance to weathering
* Good heat stability
.
Used on top of commerical roofs and used in automotive weather-stripping and seals, glass-run channel, radiator, garden and appliance hose, tubing, belts, electrical insulation, roofing membrane, geomembranes, rubber mechanical goods, plastic impact modification, thermoplastic vulcanizates and motor oil additive applications.



==========================================
Business Card __________________________________________
Cycle Heaven.......
 
Also resistant to automotive brake fluid (glycol ether based fluid).
 
Thank you for infos.

Gagar
 
EPDM to ASTM D2000 4MAA 510 A13 B13 C12 - What does it mean?
Can you advise me a named material?

the 4mAA 510 A13 etc....designates the type and class, each alpha-numberic group rates it as a different charateristic
If you have the ASTM D2000 it will explain it all.
 