Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Zinc Nickel vs Brigh Zinc

Status
Not open for further replies.

tnkayaker

Mechanical
Sep 13, 2005
32
I am looking for data that compares the salt spray results of zinc nickel with an iridecent chromate conversion with that of bright zinc. The questions I'm trying to answer are how much better is zinc nickel than bright zinc and will zinc nickel stand up to immersion in water over a 2 year period? Any help would be greatly appreciated.

Erik
 
Replies continue below

Recommended for you

A good place to start is information from engineering standards like ASTM B 633 for zinc plating and ASTM B 841 for zinc-nickel plating. For a 5 micrometer coating of Zn or Zn-Ni, the corrosion requirements are as follows:

Zn: no red rust after 96 hour salt spray test
Zn-Ni: no red rust after 500 hour salt spray test

You can also find good information from the websites of better plating companies. I have found the following to be particularly good:



 