Can anyone direct me to a data sheet or any information for Zamac 5? I have limited resources at the moment and any help would be appreciated. Thanks.
 
Replies continue below

Recommended for you

Thank you Kenneth.
 
I'm looking to use this for housing and was curious how corrosion resistent is it? Is there a similar, yet better option?
 
What type of environment will the housing be used in? As a rough generality, die cast aluminum 360 alloy or 413 alloy will offer better corrosion resistance (and less weight).
 