What is your experience with concrete core tests? What strengths do you usually find? And if it falls below requirements, do you replace the whole sections or do you retrofit it by the concept of confining the strain hence making it stronger?
I was having conversation with another engineer about this yesterday in a get together and he said it's dangerous to remove large sections of columns where core tests detect poor strength owing to the bars just bending if shoring is not perfect. Instead what is safer to do is to wrap it with retrofit to confine the strain hence increase the strength much like a cup holding sands and the sands having poor compressive strength. What is your actual experience on this?