Hi
I am trying to calculate the displacement of the top of a 14 m tall CFRP tank.
The manufacturer doesn't tell us what the Young's modulus of the material is. What is a reasonable range of values to assume?
I find conflicting information online. In the ASME-RTP-1 code, table 2A-3, it says it ranges from 0.7x10^6 psi to 1x10^6 psi (4.83 to 6.9 GPa) depending on the nominal thickness. However, I find values online that are 10 times that....
So its not clear.
Any suggestions?