Dear all,
Does anyone have the Young's Modulus for SA240-304L at 950F? Section II Part D Fig HA-3 has E value up to 800F only. I need it at 950F in order to calculate deflection for support beam. Will it be the same as 304SS that listed in Fig HA-1 ?