Dear all,
Does anyone have the Young's Modulus for SA240-304L at 950F? Section II Part D Fig HA-3 has E value up to 800F only. I need it at 950F in order to calculate deflection for support beam. Will it be the same as 304SS that listed in Fig HA-1 ?
 
Replies continue below

Recommended for you

B31.3 might have it in appendix C.
It might not be in IID due to restriction in maximum application temperature.
 
It does listed in B31.3, Appendix C, Table C-6, but it indicates for TP304, 310, 316, etc. I am not sure if it is the same for 304L. Anyone please help.
Also, I notice E value in B31.3 is 3-5% higher than Section II Part D. Do not know why.
 
Why are you looking in Fig HA-3? Table TM-1 has Young's Modulus values for Material Group G (to which 304L belongs) up to 1500°F.
 