If I made some treatment with steel or other metals, will be a change into the Yuong Module from the standar value?

thanks
 
Replies continue below

Recommended for you

Only if the material was very heavily cold worked first.
If you are measuring a change then you need to check your test methods.

= = = = = = = = = = = = = = = = = = = =
Plymouth Tube
 