Can anybody know the yield strength for P355 N between 50 deg C and 340 degree C
 
P355N does not have specified hot yield values. You should order P355NH if you need them . In that case 336,304,284,245,226,216,196 MPa for temperatures of 50,100,150,200,250,300,350 Deg. C
 