Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations JAE on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Yield Strength at Elevated Temperatures

Status
Not open for further replies.

BENDOG

Structural
Joined
Feb 9, 2007
Messages
51
Location
US
ASME II Part D (we have 2004) has tables for tensile strength and modulus of elasticity for various alloys at elevated temperatures. I'm looking for tables for yield strengths. Is that covered anywhere in ASME? If not where can I find it?
 
Maybe not your field, but you can find such info in MIL-HDBK-5 or the new MMPDS.
 
BENDOG - keep looking in Section II, Part D. You're looking for Table Y-1 (It's between Table U - where you found the tensile strength, and the Table where you found the Modulus)
 
If you have access to the Aerospace Materials Handbook, you should be able to find information on quite a few of the more exotic alloys.

MIL-HDBK-5 is another good reference (and free).

You may also look in the ASM Metals Handbook; they give you quite a bit of information on the effects of different heat treatments or processing on the mechanical properties of steels.
 
TGS4
I found the table. Thanks. I don't use this code very often and when I do I always have a hard time finding what I'm looking for.
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor