I am designing a 4 story wood structure approx. 60' x 300'. We are sitting on yazoo clay and I was wondering if anyone could help with the typical foundations seen on Yazoo (Jackson, Mississippi). We are trying to decide between piers (auger cast/drilled) with an elevated floor and crawl space or 10'-12' of over excavation then replacing with structural fill. I have read that both can still have issues. I am seeing heaving up to 30" in crawl space situations on one hand and then recommendations of up to 20' of over excavation on the other. Is there a typical system that is "tried and true"?