Feb 22, 2016 #1 sikridheeraj Mechanical Joined Jul 6, 2012 Messages 1 Location IN Do XM19 stems are more superior than SS316 & SS316L. we are having a requirement for fertilizer plant for urea application.
Do XM19 stems are more superior than SS316 & SS316L. we are having a requirement for fertilizer plant for urea application.
Feb 22, 2016 #2 EdStainless Materials Joined May 20, 2004 Messages 16,351 Location Waukesha WI USA Nitronic 50 (S20910) will have slightly better corrosion resistance than 316L, and it is often used in the cold worked condition at high strength. These alloys also have superior galling resistance, I would prefer Nit50. = = = = = = = = = = = = = = = = = = = = P.E. Metallurgy, Plymouth Tube Upvote 0 Downvote
Nitronic 50 (S20910) will have slightly better corrosion resistance than 316L, and it is often used in the cold worked condition at high strength. These alloys also have superior galling resistance, I would prefer Nit50. = = = = = = = = = = = = = = = = = = = = P.E. Metallurgy, Plymouth Tube