Nov 19, 2020 #1 rajnad Materials Joined Nov 7, 2011 Messages 7 Location AE Hi Friends, I have a query. Is it possible to have the below properties in a Xm-19 Bar ? YS ≥ 850 Mpa TS ≥ 1000 Mpa Kv ≥ 45 (196°C) In case the bar is strain hardened, the required Kv properties would not be achievable ? Thanks
Hi Friends, I have a query. Is it possible to have the below properties in a Xm-19 Bar ? YS ≥ 850 Mpa TS ≥ 1000 Mpa Kv ≥ 45 (196°C) In case the bar is strain hardened, the required Kv properties would not be achievable ? Thanks
Nov 19, 2020 #2 SwinnyGG Mechanical Joined Jan 22, 2016 Messages 2,599 Location US You should contact your vendor for this material and ask them these questions directly. Upvote 0 Downvote
Nov 20, 2020 #3 LUengineer Materials Joined Dec 18, 2019 Messages 2 Location US Looks reasonable depending on size and any other potential requirements. You can reach out to Carpenter Technology. Upvote 0 Downvote
Looks reasonable depending on size and any other potential requirements. You can reach out to Carpenter Technology.
Nov 20, 2020 #4 EdStainless Materials Joined May 20, 2004 Messages 16,364 Location Waukesha WI USA I have only seen those properties up to about 1.5" diameter. You know that you could buy some pieces off the shelf to test? Aqumet.com This ia used as boat prop shafting and you could buy short pieces. = = = = = = = = = = = = = = = = = = = = P.E. Metallurgy, consulting work welcomed Upvote 0 Downvote
I have only seen those properties up to about 1.5" diameter. You know that you could buy some pieces off the shelf to test? Aqumet.com This ia used as boat prop shafting and you could buy short pieces. = = = = = = = = = = = = = = = = = = = = P.E. Metallurgy, consulting work welcomed