May 3, 2016 #1 avsrao81 Mechanical Joined May 3, 2016 Messages 1 Location IN HOW TO ACHIEVE FATT VALUES FOR X20Cr13 MATERIAL? DOES CHEMISTRY PLAY A ROLE OR HEAT TREATMENT? EXPERIENCES MAY PLEASE BE SHARED.
HOW TO ACHIEVE FATT VALUES FOR X20Cr13 MATERIAL? DOES CHEMISTRY PLAY A ROLE OR HEAT TREATMENT? EXPERIENCES MAY PLEASE BE SHARED.
May 3, 2016 #2 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US This material is similar to 420 stainless and heat treatment (quench and temper) would be the controlling factor for FATT values. The carbon content will effect the upper and lower shelf peak values. Upvote 0 Downvote
This material is similar to 420 stainless and heat treatment (quench and temper) would be the controlling factor for FATT values. The carbon content will effect the upper and lower shelf peak values.