HOW TO ACHIEVE FATT VALUES FOR X20Cr13 MATERIAL? DOES CHEMISTRY PLAY A ROLE OR HEAT TREATMENT?
EXPERIENCES MAY PLEASE BE SHARED.
 
Replies continue below

Recommended for you

This material is similar to 420 stainless and heat treatment (quench and temper) would be the controlling factor for FATT values. The carbon content will effect the upper and lower shelf peak values.
 