mog69
Mining
- Mar 12, 2006
- 57
Does anybody recognise this designation of Aluminium?
I believe it was referenced in BS 1476, but this standard is now obsolete and I didn't keep my copy !
The reference I have is on a drawing which is in poor condition and difficult to read, so it could be HE 15 and the suffix could be "W" rather than "V".
If anybody recognises it, could they either let know composition / mech properties, or what the current equivalent would be?
I believe it was referenced in BS 1476, but this standard is now obsolete and I didn't keep my copy !
The reference I have is on a drawing which is in poor condition and difficult to read, so it could be HE 15 and the suffix could be "W" rather than "V".
If anybody recognises it, could they either let know composition / mech properties, or what the current equivalent would be?