Hi all,
As per 15614-1, will a WPQR done with 304 base material, cover welding 316 base material.

316 filler wire used.
 
Replies continue below

Recommended for you

It'll cover all aust. stainless steels in gr. 8.
It's up to you to make sure they're weldable with the exact same filler metal, when writing WPS'ses...
 