bhart192
Civil/Environmental
- Feb 6, 2006
- 81
AWS d1.1 section 4 ,table 4.1 ,I need to qualify a wps for making a single bevel joint in a tube section ,no backing bar welded from 1 side,I work with ASME IX more than AWS ,from table 4.1 it appears we would have to weld the coupon used for mech. testing in position . ASME IX does not require any particular position when making weld samples to qualify a WPS,am I reading table 4.1 correct that I would have to make the sample joint in the 6g position to qualify the WPS for all postions ,I can understand position being a esential var. for a welder performance test but not to qualify a WPS. my understanding of wps qualification testing verify's the joints ability to perform up to the base metal standards.