I have two qualified wps/pqr API 1104 which comprise API 5L-B to API 5L-B and API 5L-X52 to API 5L-X52. I would like to joining API 5L-B to API 5L-X52. May I to used these wps/pqr without requalified? the others essential variables is still comply with API 1104.
 