timsch
Mechanical
- Oct 27, 2009
- 194
I've created WPS's for butt joints where there is a buttering layer on one end of a base metal that gets PWHT and then welded to a 2nd base metal that needs no PWHT. ASME BPVC SEC IX, QW-283 seems to be written with this orientation in mind; at least when I read QW-283.2.
I now have a job where I need to build up a 4" x 6" x 3/16" alloy 625 butter pad on the OD of a P5 pipe to then weld temperature sensors to. What test specimen orientation should be used here? Treat it like a butt weld with a 3/16 butter layer and then the weld with the 2nd base metal?
Note: this is a repost from another forum
I now have a job where I need to build up a 4" x 6" x 3/16" alloy 625 butter pad on the OD of a P5 pipe to then weld temperature sensors to. What test specimen orientation should be used here? Treat it like a butt weld with a 3/16 butter layer and then the weld with the 2nd base metal?
Note: this is a repost from another forum