Feb 11, 2014 #1 Jeldon Chemical Joined May 20, 2013 Messages 25 Location BR Qualification of WPS by Section 4, with different thicknesses 1/2'' x 2'', which will be the qualified range?
Qualification of WPS by Section 4, with different thicknesses 1/2'' x 2'', which will be the qualified range?
Feb 11, 2014 1 #2 gtaw Structural Joined Feb 10, 2006 Messages 1,988 Location US It is based on the thinner of the two members joined if you are working to D1.1. Best regards - Al Upvote 0 Downvote