MDMT for vessel is -50°F for design pressure. There one more condition other than design pressure (pressure less than design pressure) which needs MDMT of -58°F.
Using reduction ratio UCS-66 base metal needs to be impact tested at -50°F and not at -58°F.
Can we take reduction for impact testing of WPS and PQR? Can we impact test WPS and PQR at -50°F OR we have to impact WPS and PQR at -58°F?
Thanks
Dinesh
Using reduction ratio UCS-66 base metal needs to be impact tested at -50°F and not at -58°F.
Can we take reduction for impact testing of WPS and PQR? Can we impact test WPS and PQR at -50°F OR we have to impact WPS and PQR at -58°F?