Dear all
I have a welding procedure qualification (test coupon 17.1mm)with two different process GTAW with 2 layers of 5mm and 12.1mm with SMAW.
i want to replace the GTAW process by SMAW process.What is the range of qualification of this welding procedure qualification according ASME lX???
I have a welding procedure qualification (test coupon 17.1mm)with two different process GTAW with 2 layers of 5mm and 12.1mm with SMAW.
i want to replace the GTAW process by SMAW process.What is the range of qualification of this welding procedure qualification according ASME lX???