Hi,
I'm looking for an adhesive to hold the wire in place. this adhesive has to be at 2500F , don't give off any gas, and has to cure fast. do you have any suggestions.
 
Welded clips.

Except few metals themselves retain strength at that high a temperature.

Screw it down with Ti mounts and screws or nuts.
 
we don't want to weld. that wire is wrapping the cylinder. we want to glue the wire
 
Check out ceramic adhesives.