Feb 2, 2016 #1 ebirinci Electrical Joined Dec 14, 2015 Messages 11 Location US Hi, I'm looking for an adhesive to hold the wire in place. this adhesive has to be at 2500F , don't give off any gas, and has to cure fast. do you have any suggestions.
Hi, I'm looking for an adhesive to hold the wire in place. this adhesive has to be at 2500F , don't give off any gas, and has to cure fast. do you have any suggestions.
Feb 2, 2016 #2 racookpe1978 Nuclear Joined Feb 1, 2007 Messages 5,995 Location US Welded clips. Except few metals themselves retain strength at that high a temperature. Screw it down with Ti mounts and screws or nuts. Upvote 0 Downvote
Welded clips. Except few metals themselves retain strength at that high a temperature. Screw it down with Ti mounts and screws or nuts.
Feb 2, 2016 Thread starter #3 ebirinci Electrical Joined Dec 14, 2015 Messages 11 Location US we don't want to weld. that wire is wrapping the cylinder. we want to glue the wire Upvote 0 Downvote
Feb 2, 2016 #4 ornerynorsk Industrial Joined Feb 5, 2002 Messages 3,198 Location US Check out ceramic adhesives. It is better to have enough ideas for some of them to be wrong, than to be always right by having no ideas at all. Upvote 0 Downvote
Check out ceramic adhesives. It is better to have enough ideas for some of them to be wrong, than to be always right by having no ideas at all.
Feb 2, 2016 Thread starter #5 ebirinci Electrical Joined Dec 14, 2015 Messages 11 Location US thank you Upvote 0 Downvote
Feb 2, 2016 #6 EdStainless Materials Joined May 20, 2004 Messages 16,374 Location Waukesha WI USA We used these for anchoring lead wires on resistance heating elements http://www.sauereisen.com/ProductIndex.aspx = = = = = = = = = = = = = = = = = = = = P.E. Metallurgy, Plymouth Tube Upvote 0 Downvote
We used these for anchoring lead wires on resistance heating elements http://www.sauereisen.com/ProductIndex.aspx = = = = = = = = = = = = = = = = = = = = P.E. Metallurgy, Plymouth Tube
Feb 3, 2016 Thread starter #7 ebirinci Electrical Joined Dec 14, 2015 Messages 11 Location US I found ceramic adhesive http://www.cotronics.com/vo/cotr/ca_fastset.htm this is what I was looking for Upvote 0 Downvote
I found ceramic adhesive http://www.cotronics.com/vo/cotr/ca_fastset.htm this is what I was looking for