What you may be looking was called "excelsior" and was made from shaved aspen, pine or other softwoods. It was also used to fill upholstered furniture and stuffed animals (toys).
I think there are still people making it, but I do not have any details of how it is made. It may be a by-prodcut from some other manufacturing process.