Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations TugboatEng on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

wire size to mig weld

Status
Not open for further replies.

CMAF

Automotive
Joined
Jul 8, 2001
Messages
1
Location
US
I am putting a new Quarter panel on a 2000,gmc piick up.
I need to know what wire size to use.I currently have 023 wire.I am useing Argon gas.Also will 30 wire work as well?
 
Automotive manufactures in Australia use 1.2 mm wire in the robot welders and 0.9 mm wire for the hand welders with a argon CO2 mix.
 
Dear collegue

It is very common use with C,S, Shielded Gas as CO2 and Diameters Wires 0.035 & .045" .with S.S use Ar or Ar+02and the same Diameters.
Regards
Tecnico1948